Combined Carbonation and Water Curing Improves CO2-Injected Concrete Density and Strength
bioengineer.orgA new study in Bioengineer.org examines how different curing regimes affect CO2-injected concrete. Researchers mixed CO2 into fresh mortar and then applied either carbonation curing, water curing, or a combined carbonation-water curing. The combined method gave the lowest porosity and highest compressive strength across multiple mix designs, outperforming water-cured samples by up to 26.6 percent in C20 concrete. The study also used digital image correlation to track crack formation, showing that the combined curing reduces defect-driven strain concentrations. The work addresses a key challenge: CO2 injection hurts workability by triggering rapid calcium silicate reactions. The combined curing, with an initial water bath followed by carbonation, lets hydration build a strong matrix before carbonation fills remaining pores. This could make CO2 storage in concrete more practical, but the paper notes that high-strength mixes still suffer from rheological stiffening. Real-world scale-up and cost remain open questions, especially for precast vs. cast-in-place applications.